| Specification data | |||
| MIG Function | ARC Function | Optional LIFT TIG Function | |
| Power supply voltage(V) | 110V/220V 50/60Hz | ||
| Effective Current(A) | 38.7A@110V 26.3A@220V |
38.7A@110V 26.3A@220V |
27.8A@110V 18.5A@220V |
| Rated Imput Power(kW) | 5.5kW@110V 7.48kW@220V |
5.5kW@110V 7.48kW@220V |
3.9kW@110V 5.2kW@220V |
| Rated Input Current(A) | 50A@110V 34A@220V |
50A@110V 34A@220V |
36A@110V 24A@220V |
| Duty cycle(40℃ 10min) | 60%@160A, 100%@123A @110V 60%@205A, 100%@158A @220V |
60%@145A, 100%@112A @110V 60%@180A, 100%@139A @220V |
60%@160A, 100%@123A @110V 60%@205A, 100%@158A @220V |
| No-Load Voltage(V) | 62 V | ||
| Welding Current Range(A) | 30-160A@110V 30-205A@220V |
20-145A@110V 20-180A@220V |
20-160A@110V 20-205A@220V |
| Welding Voltage Range(V) | 15.5-22.0V@110V 15.5-24.2V@220V |
20.8-25.8V@110V 20.8-27.2V@220V |
10.8-16.4V@110V 10.8-18.2V@220V |
| Welding Wire Size Range | 0.8mm&0.9mm (.030″ & .035″ ) carbon steel wire 0.9mm&1.2mm (.035″ & .045″ ) aluminum wire |
7018/6011 electrodes up to 3.0mm(1/8″)@110V, 4.0mm(5/32″)@220V |
/ |
| Maximum Wire Feed Speed | 15m / min | / | / |
| Operating Temp | -10℃- 50℃ | ||
| Compatible Metal | Carbon Steel / Aluminum / Stainless Steel | ||
| Product size(L×W×H) | 460×205×300 mm (18.11×8.07×11.81 in.) |
||
| Product weight | 10.4 kg (22.93 lbs) | ||
| Protection class | IP21S | ||

YesWelder confidently offers a three-month free trial sale support service to help distributors test the market without any stock issues.

Every YesWelder product goes through a complete quality control inspection to ensure that the final products are safe, compliant, and meets consumer demands.

YesWelder invests in all the advertising media channels to optimize the sales funnel, and help our distributors to expand their market easily.

Our goal is to provide our customers with dependable aftermarket support, including but not limited to product liability insurance, a one-year warranty, and after-service maintenance.